Thermoforming wall thickness variation appears when a heated sheet stretches unevenly into a cup or tray. The base, corners, sidewalls and rim do different work during forming. To troubleshoot a weak region, make a thickness map for each tool cavity and compare it with the product's performance requirement.
Do not infer the thickness of a corner from an easy-to-reach flat wall.
Why a formed part thins out
The heated sheet has a limited amount of material to cover a larger three-dimensional surface. As it stretches, some regions become thinner. Contact with the plug and mold, temperature differences and the sequence of forming can redistribute material.
Research by Martin and Duncan found that plug geometry affects the wall-thickness distribution. The finding is a process principle, not a setting that applies to every cup.
Identify the intended material, original sheet, draw geometry and critical use conditions before deciding where to measure. A thin point is important when it controls strength, barrier or sealing performance; a thickness map provides the evidence for that decision.
Map corners, sidewalls and base
Mark the rim, upper wall, lower wall, corner radius and base on a drawing or photograph. If the tray has different corner designs, label each one. Keep the orientation and part position consistent across measurements.
Record each cavity separately so a localized tool problem is not hidden by a combined average.
For a deep cup, check both the base center and the transition into the sidewall. The location of the minimum may shift with process conditions. A point map should be revised when the tool, sheet or plug changes.
Questions about a model or a test? Email Amy Zhao, Export Manager, at info@halleffectthicknessgauge.com.
Process variables to investigate
Sheet temperature, plug shape, plug temperature, displacement and contact friction can affect material distribution. McCool and Martin's experimental work identified several of these as influential in plug-assisted thermoforming. A Thermoforming Division technical article likewise discusses plug roughness and the resulting thickness pattern.
The direction of the effect depends on the material and geometry, so use a controlled trial rather than a generic rule such as “more heat always gives thicker corners.”
Change one planned factor at a time where possible and keep the same measurement map. Compare both the thinnest region and the variation across cavities. A change that improves the base can still worsen a sidewall.
Measure difficult areas carefully
The KHT thickness-gauge homepage introduces a Hall-effect gauge for non-magnetic wall and base measurements. The available capability record does not establish that the probe and target can reach every thermoformed cup or tray corner. Before specifying a non-destructive method, check opening size, corner curvature, target-ball seating and probe orientation on actual samples.
If a location is inaccessible, use an agreed alternative method and label the results separately.
Do not press a flexible wall into a different shape to make the probe fit unless the measurement method accounts for that deformation. A repeatable contact condition matters more than taking a larger number of inconsistent readings.
Keep a useful tool-by-tool record
For each cavity, record tool ID, material and sheet lot, process settings, measurement locations and individual values. Attach the location map to the report. Trend the weakest region over production time. The same logging fields are described in our wall thickness inspection record guide.
If one cavity drifts, check tool wear, heat distribution and plug condition before changing all cavities.
Further reading and methods
- Martin and Duncan on plug design, Polymer Engineering & Science
- McCool and Martin on process parameters, Polymer Engineering & Science
- SPE Thermoforming Division article on plug roughness
Frequently asked questions
Is the base always the thinnest part?
No. The pattern changes with tool geometry and process conditions. Measure the actual part.
Can a bottle-wall gauge measure every cup corner?
Not automatically. Confirm access and target seating on the specific cup or tray before relying on the reading.
Review a thickness-mapping setup with KHT
We sell direct from our factory, so you work directly with our factory team.
Questions about a model or a test? Email Amy Zhao, Export Manager, at info@halleffectthicknessgauge.com. Share a drawing, material details and the measurement points with your requirements. Ask KHT to confirm the proposed configuration.